Welcome to the Australian Ford Forums forum.

You are currently viewing our boards as a guest which gives you limited access to view most discussions and inserts advertising. By joining our free community you will have access to post topics, communicate privately with other members, respond to polls, upload content and access many other special features without post based advertising banners. Registration is simple and absolutely free so please, join our community today!

If you have any problems with the registration process or your account login, please contact us.

Please Note: All new registrations go through a manual approval queue to keep spammers out. This is checked twice each day so there will be a delay before your registration is activated.

Go Back   Australian Ford Forums > General Topics > The Pub

The Pub For General Automotive Related Talk

Reply
 
Thread Tools Display Modes
Old 25-08-2009, 08:49 PM   #1
Kowalski
FF.Com.Au Hardcore
 
Kowalski's Avatar
 
Join Date: May 2005
Location: Geelong
Posts: 980
Default Panel Bonding Glue/Adhesive??

As the title indicates, has anyone here used it?
Is it any good?
Where would you get it?
Is it expensive?
That's probably enough questions for now

Kowalski is offline   Reply With Quote Multi-Quote with this Post
Old 25-08-2009, 08:55 PM   #2
yift
FF.Com.Au Hardcore
 
Join Date: Oct 2006
Posts: 1,819
Technical Contributor: For members who share their technical expertise. - Issue reason: Countless sensible, accurate mechanical advice on all things Falcon and Territory. 
Default

is it the same stuff the car mufacturers are using on turrents etc?
yift is offline   Reply With Quote Multi-Quote with this Post
Old 25-08-2009, 09:33 PM   #3
Smoke Pursuit
FF.Com.Au Hardcore
 
Join Date: Dec 2004
Posts: 22,922
Valued Contributor: For members whose non technical contributions are worthy of recognition. - Issue reason: DASH/bfiipursuit has been alot of help over the years I have frequented this forum, lots of thoughtful and informed posts, very much a valued contributor. 
Default

Sikaflex or something else?
__________________
2022 RAM Laramie 5.7
2023.50 Ranger Wildtrak 3.0 V6 Premium Pack
2024 Everest Sport 3.0 V6 Touring Pack
2024.50 Mustang Darkhorse 6M Blue Ember + Appearance pack ETA Jan 25.
Smoke Pursuit is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 12:14 AM   #4
svo347
AFF's 1st DM.......
 
svo347's Avatar
 
Join Date: Dec 2004
Location: Wha???... There is only 2 states 2 be in.. WA or Drunk..
Posts: 6,200
Default

+1 for sikaflex
__________________
FORD GIVING POWER TO THE PEOPLE
Alloy headed 347ci EDXR8
13.21 @107.7mph
Quote:
Originally Posted by zetec
I know what lengths they go to to ensure it's more than just a Ford sticker on the part. Ford doesn't throw it's name on anything for a quick buck.
06 Turbo Terri AWD 6 sp in Neo with stuff i didnt even need, side steps,15.2 inch roof mounted DVD,Pioneer $tezza,Selby 30/18mm swaybars,debunged,100 cpsi Ballistic cat,Plazmaman under battery Cai injectors 14/lb boost,ZF tuned,Xtreme's magic. :
svo347 is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 05:32 AM   #5
gazza414
Regular Member
 
Join Date: Dec 2008
Posts: 297
Default

There are various grades so be sure to choose wisely..also be very careful of the preparation too.....
__________________
217.443mph on the Salt..Lake Gairdner
gazza414 is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 06:26 AM   #6
platinumXR
IWCMOGTVM Club Supporter.
 
platinumXR's Avatar
 
Join Date: Nov 2008
Location: Sydney
Posts: 891
Default

I'm partial to Henkel Terostat...good fillers & bonders. Better than Sika I reckon. I have been reliably informed that Ford use Teroson too.

Prices aren't too bad, try Bursons - although they mainly carry Sika from memory. Google panel beating supplies etc. and see what comes up.
__________________


Toys:
2017.5 LZ Focus RS, Magnetic Grey my new pocket rocket
2008 BF2 RTV Ute
1993 EB2 S-XR8 Sedan, Platinum, manual (now sold)
1975 XB Fairmont GS Sedan, Tropic Gold...or Starlight Blue...not sure yet...(SOLD)
platinumXR is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 06:54 PM   #7
Kowalski
FF.Com.Au Hardcore
 
Kowalski's Avatar
 
Join Date: May 2005
Location: Geelong
Posts: 980
Default

Just to clarify, this is the glue that is now used to bond panels.
Intending to maybe use it to bond some replacement quarters to the XP van rather than welding. Is this the same stuff you guys are talking about?
Kowalski is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 06:56 PM   #8
yift
FF.Com.Au Hardcore
 
Join Date: Oct 2006
Posts: 1,819
Technical Contributor: For members who share their technical expertise. - Issue reason: Countless sensible, accurate mechanical advice on all things Falcon and Territory. 
Default

sikaflex wont do it but the stuff i was on about there is aspecial process from memory you need some special high temp oven for it. not worth it weld it, lead wipe it and spray it is my opinion.
yift is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 07:06 PM   #9
platinumXR
IWCMOGTVM Club Supporter.
 
platinumXR's Avatar
 
Join Date: Nov 2008
Location: Sydney
Posts: 891
Default

Quote:
Originally Posted by Kowalski
Just to clarify, this is the glue that is now used to bond panels.
Intending to maybe use it to bond some replacement quarters to the XP van rather than welding. Is this the same stuff you guys are talking about?
Well, it's what I am on about:

__________________


Toys:
2017.5 LZ Focus RS, Magnetic Grey my new pocket rocket
2008 BF2 RTV Ute
1993 EB2 S-XR8 Sedan, Platinum, manual (now sold)
1975 XB Fairmont GS Sedan, Tropic Gold...or Starlight Blue...not sure yet...(SOLD)
platinumXR is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 07:09 PM   #10
Yellow_Festiva
Where to next??
 
Yellow_Festiva's Avatar
 
Join Date: Oct 2006
Location: Sydney
Posts: 8,893
Default

When I visited the PRB factory in Chullora they used an adhesive that looked a bit like an epoxy resin. Was a 2 part glue, and was applied direct from whatever canister it was stored in, and they had about 30 min before the product set.

Don't remember them mentioning any special oven etc. They used it to glue the joins on the composite fibre Clubmans. After they were glued, they were then reinforced with steel fixtures and rivets.

The stuff was so strong that if you used it to glue 2 panels together, pulling them apart would shear the steel before the join parted.

As for the name, sorry can't help you.

I'm sure it is a similar glue to what panel beaters use to glue new roof sections onto repaired cars. When the Festiva went in for hail damage, the roof was removed, the new one was glued back in, then the original spot welds were re-done.
Yellow_Festiva is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 07:39 PM   #11
Kowalski
FF.Com.Au Hardcore
 
Kowalski's Avatar
 
Join Date: May 2005
Location: Geelong
Posts: 980
Default

Thanks guys,
platinumXR, I have a couple of questions for you......
Can the stuff you've suggested be readily found?
Does it need any special tools/oven/process? Or could I use it at home?
Thanks again
Kowalski is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 07:45 PM   #12
svo347
AFF's 1st DM.......
 
svo347's Avatar
 
Join Date: Dec 2004
Location: Wha???... There is only 2 states 2 be in.. WA or Drunk..
Posts: 6,200
Default

Sorry mate i was thinking about applying body kits to cars etc..
__________________
FORD GIVING POWER TO THE PEOPLE
Alloy headed 347ci EDXR8
13.21 @107.7mph
Quote:
Originally Posted by zetec
I know what lengths they go to to ensure it's more than just a Ford sticker on the part. Ford doesn't throw it's name on anything for a quick buck.
06 Turbo Terri AWD 6 sp in Neo with stuff i didnt even need, side steps,15.2 inch roof mounted DVD,Pioneer $tezza,Selby 30/18mm swaybars,debunged,100 cpsi Ballistic cat,Plazmaman under battery Cai injectors 14/lb boost,ZF tuned,Xtreme's magic. :
svo347 is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 07:58 PM   #13
platinumXR
IWCMOGTVM Club Supporter.
 
platinumXR's Avatar
 
Join Date: Nov 2008
Location: Sydney
Posts: 891
Default

Quote:
Originally Posted by Kowalski
Thanks guys,
platinumXR, I have a couple of questions for you......
Can the stuff you've suggested be readily found?
Does it need any special tools/oven/process? Or could I use it at home?
Thanks again

Nup, any good panelbeating suppliers should have it or be able to get it easily - Google is your friend.

I just use a caulking gun for mine (9320 - 4 In One filler) and most are air dry and you can weld over them. The bonders are stronger than welding as well, I know as I have seen first hand.

Give Peter Weinert - Business Development Specialist (Auto Body) from Henkel Aust. a call on 0418364180 (Seven Hills, Sydney) if you need any expert technical advice.

There's some tecnical data sheets available at: http://www.loctite.com.au/cps/rde/xc...4_AUS_HTML.htm just choose the product number, eg: 9320 and just type it in.
__________________


Toys:
2017.5 LZ Focus RS, Magnetic Grey my new pocket rocket
2008 BF2 RTV Ute
1993 EB2 S-XR8 Sedan, Platinum, manual (now sold)
1975 XB Fairmont GS Sedan, Tropic Gold...or Starlight Blue...not sure yet...(SOLD)
platinumXR is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 08:01 PM   #14
platinumXR
IWCMOGTVM Club Supporter.
 
platinumXR's Avatar
 
Join Date: Nov 2008
Location: Sydney
Posts: 891
Default

I just looked up 9220 and it is air curing but you can heat it up to cure faster if necessary.

Honestly, if you are still unsure: give Peter a call.
__________________


Toys:
2017.5 LZ Focus RS, Magnetic Grey my new pocket rocket
2008 BF2 RTV Ute
1993 EB2 S-XR8 Sedan, Platinum, manual (now sold)
1975 XB Fairmont GS Sedan, Tropic Gold...or Starlight Blue...not sure yet...(SOLD)
platinumXR is offline   Reply With Quote Multi-Quote with this Post
Old 26-08-2009, 08:06 PM   #15
Kowalski
FF.Com.Au Hardcore
 
Kowalski's Avatar
 
Join Date: May 2005
Location: Geelong
Posts: 980
Default

Thanks mate, massive help!
Kowalski is offline   Reply With Quote Multi-Quote with this Post
Reply


Forum Jump


All times are GMT +11. The time now is 03:43 PM.


Powered by vBulletin® Version 3.8.5
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Other than what is legally copyrighted by the respective owners, this site is copyright www.fordforums.com.au
Positive SSL